By Marcus - 3/1/2020 10:18:44 AM

Hi
i need a new filter element for the vacuum pump EC.4 ("exhaust filter" DVP 1801046). it is full of oil due i ran the pump a few hours with a leak in my bag.
Can you supply it?
As for the GC50 i´m interested how if it is possible to repair little imperfections after the part is ready (weeks or months later). GC50 will not bond to itself and the epoxy part is hardened so it won´t bond to the epoxy part.

regards

By Warren (Staff) - 3/3/2020 9:21:55 AM

We can supply a filter no problem.  If you email or phone us we can add it to another order or create an order for you especially.