Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Other
»
Base coat.
Base coat.
Post Reply
Like
8
Base coat.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Alex1981
A
Alex1981
posted 6 Years Ago
ANSWER
HOT
Topic Details
A
Group: Forum Members
Posts: 4,
Visits: 23
Hi. What I have to use to stick carbon fibre to the part (plastic skinning ) car interior parts. Try it to use base coat but looks to me not stick well. Used mix 100:40. I am beginner in this and try in do my first car interior parts
Thank you
Reply
Like
8
Reply
oekmont
oekmont
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 550,
Visits: 27K
In my opinion the best product for this is a polyurethane basecoat. Polyurethanes have much better bonding characteristics in general.
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Base coat.
Alex1981
-
6 Years Ago
Most plastics are pretty difficult for laminating resins to bond to, so there is no real solution. Extremely rough sanding with a 40 or 60 grit paper plus scoring the plastic with a sharp knife will....
Hanaldo
-
6 Years Ago
In my opinion the best product for this is a polyurethane basecoat. Polyurethanes have much better bonding characteristics in general.
oekmont
-
6 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search