By Alex1981 - 2/24/2020 9:12:16 AM

Hi. What I have to use to stick carbon fibre to the part (plastic skinning ) car interior parts. Try it to use base coat but looks to me not stick well. Used mix 100:40.  I am beginner in this and try in do my first car interior  parts
Thank you  
By oekmont - 2/25/2020 8:09:51 AM

In my opinion the best product for this is a polyurethane basecoat. Polyurethanes have much better bonding characteristics in general.