	Group: Forum Members 	        
    Posts: 2.5K, 
    Visits: 28K 
    
 
          
		     | 
				                       
                 
                
                    
			            Most plastics are pretty difficult for laminating resins to bond to, so there is no real solution. Extremely rough sanding with a 40 or 60 grit paper plus scoring the plastic with a sharp knife will give you the best chance, but there's a good chance the carbon will delaminate and bubble over time, especially with the temperature changes interior components will see.
  Not really something I would advise doing, it's just not very reliable.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |