Resin cure and heat dissipation.


Author
Message
Daveb
D
posted 6 Years Ago Merged HOT
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 4, Visits: 5
Hi,

I am making a resin river table that is 47mm thick. I am planning on pouring about 10mm at a time to avoid as many air bubbles as possible.

The question I have is this. If I let each 10mm pour get to the B cure stage before pouring the next layer, will I have a problem with heat build up, or would most of the heat have already dissipated by the time it gets to the B cure stage?

Any help would be appreciated.

Many Thanks

DB