By Daveb - 2/18/2020 11:55:31 AM
Hi,
I am making a resin river table that is 47mm thick. I am planning on pouring about 10mm at a time to avoid as many air bubbles as possible.
The question I have is this. If I let each 10mm pour get to the B cure stage before pouring the next layer, will I have a problem with heat build up, or would most of the heat have already dissipated by the time it gets to the B cure stage?
Any help would be appreciated.
Many Thanks
DB
|
By Daveb - 2/20/2020 12:49:36 PM
Matt,
Thanks very much for the reply. I will seal coat the lot and key it before doing the main pours I think.
Thanks very much.
DB
|
|