ABS is fine.  it will slightly etch the surface which helps. Key the surface and give it a good clean and degrease and you should be good for bonding. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
IanK
I
Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)
Group: Forum Members
Posts: 1, Visits: 1
Hi,

I've got a pair of these

https://parts.westfield-sportscars.co.uk/index.php?route=product/product&product_id=573&search=cycle+wing&description=true

Plastic cycle wings fitted to a kit car. One has developed a crack near to the mounting hole. I think they are 'ABS'

Would your Vuduu glue be suitable to repair it by sticking another piece of ABS under the cracked area?

https://www.easycomposites.co.uk/solution-mw-wax-gelcoat-additive

Thanks,

Ian