Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
General Composites Discussion
ABS and Vuu doo glue
http://www.talkcomposites.com/Topic34810.aspx
By IanK
-
2/10/2020 10:36:00 AM
Hi,
I've got a pair of these
https://parts.westfield-sportscars.co.uk/index.php?route=product/product&product_id=573&search=cycle+wing&description=true
Plastic cycle wings fitted to a kit car. One has developed a crack near to the mounting hole. I think they are 'ABS'
Would your Vuduu glue be suitable to repair it by sticking another piece of ABS under the cracked area?
https://www.easycomposites.co.uk/solution-mw-wax-gelcoat-additive
Thanks,
Ian
By Warren (Staff)
-
2/12/2020 10:35:43 AM
ABS is fine. it will slightly etch the surface which helps. Key the surface and give it a good clean and degrease and you should be good for bonding.