A lot of cases where "grip patches" are added can be done by adding very fine sand or grit to the mix to make a rougher surface in those areas. However, on a clear resin such as this, it will compromise clarity heavily so may not be an ideal solution. Alternatively, you can get stick on grip patches specifically for baths. Some are black, some are clear "ish".