Hi. My name is Alex and I am new in this. I would like to learn how to do skinning car parts and do some  parts from carbon fibre. I would like to start from skinning parts first. My quastion: 
1. What is best resin for skinning parts? Do I need black background for parts? ( original parts are silver) I have f30 bmw. And some interior parts are silver.
2.Can I use vacuum system to do skinning? If es what kind of materials I need and any advise for new person in this things.
Reason for skinning: all parts have some mounting clicks. 
Thank you

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search