Vacuum Pump leaking oil into the bagging pipe
Vacuum Pump leaking oil into the bagging pipe
Post Reply
Like
6
Vacuum Pump leaking oil into the bagging pipe
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
bhanu prakash
bhanu prakash
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 8
Sir/Ma'am,
I have a vacuum pump (model
. Recently, I have been facing the issue of vacuum pump oil leaking into the vacuum bagging pipe. I am attaching the photos below. Kindly help me understand and solve this issue.
Bhanu
Attachments
1.jpeg
(
387 views,
58.00 KB
)
2.jpeg
(
391 views,
75.00 KB
)
3.jpeg
(
340 views,
48.00 KB
)
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Vacuum Pump leaking oil into the bagging pipe
bhanu prakash
-
6 Years Ago
model name is ECVP425
bhanu prakash
-
6 Years Ago
This could happen if you leave the tap on the pump open after you've switched-off the pump, as the vacuum inside the catch pot or vacuum line would draw the oil from the pump. it's only likely to be...
MarkMK
-
6 Years Ago
Bingo ^ These older style pumps don't have a one-way valve on the inlet, so if you don't shut it off afterwards then you essentially 'infuse' the oil out of the pump. The new pumps from EC have a....
Hanaldo
-
6 Years Ago
Thank you, Mark and Hanaldo for the advice. It works.
bhanu prakash
-
6 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search