Sir/Ma'am,
I have a vacuum pump (modelSmile. Recently, I have been facing the issue of vacuum pump oil leaking into the vacuum bagging pipe. I am attaching the photos below. Kindly help me understand and solve this issue.

Bhanu

Attachments
1.jpeg (264 views, 58.00 KB)
2.jpeg (217 views, 75.00 KB)
3.jpeg (225 views, 48.00 KB)
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Bingo ^ 

These older style pumps don't have a one-way valve on the inlet, so if you don't shut it off afterwards then you essentially 'infuse' the oil out of the pump.

The new pumps from EC have a one way valve built in so this isn't an issue.