Stored correctly, the shelf life on all of the GLassCast Epoxies is 12 months; realistically and because we get through so much), you should have 12 months from the date of dispatch albeit generally, the resin side will last much longer than this , the hardener will degrade faster.
bclark
b
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 1, Visits: 3
Can you advise me what shelf life I might expect for the GlassCast 50 ?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search