By bclark - 1/7/2020 9:27:43 AM
Can you advise me what shelf life I might expect for the GlassCast 50 ?
|
By Rich (Staff) - 1/7/2020 5:14:51 PM
Hi bclarke,
Stored correctly, the shelf life on all of the GLassCast Epoxies is 12 months; realistically and because we get through so much), you should have 12 months from the date of dispatch albeit generally, the resin side will last much longer than this , the hardener will degrade faster.
|
|