+x Martin Fraser - 11/13/2019 6:52:15 PM+x James Hurd - 11/13/2019 2:43:58 PMLooks like a wet lay up. As there is a cut out for the canopy could be a tricky spot.. This area would be very hard to seal up for an infusion due to not having a full flange like what around the rest of the fuse.. How Did you make the moulds? Was it with the Uni mould system from Ez composites? Hi James,The moulds were made using epoxy tooling gel coat, epoxy and glass. If I was to vacuum it, I was thinking of bagging it. What do you think?Cheers, Marty
+x James Hurd - 11/13/2019 2:43:58 PMLooks like a wet lay up. As there is a cut out for the canopy could be a tricky spot.. This area would be very hard to seal up for an infusion due to not having a full flange like what around the rest of the fuse.. How Did you make the moulds? Was it with the Uni mould system from Ez composites?