Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Zhengning Zhang,

It sounds like interesting research but that's a very specialist pre-form and not something that we could source our manufacture for you. Specifically, to be able to weave a pre-form like this would require specialist weaving equipment which we don't have.

Sorry we can't be more help and I wish you all the best with your project.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Zhengning Zhang
Zhengning Zhang
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 13
Hi
I am a Y3 university student in Liverpool. This year I have an individual project about adhesive composite T-joints. It is a project started at University of Michigan in U.S. My supervisor brought it to U.K. Because of short of the material of the carbon fiber fre-form, we need your help.

 The company, which made the pre-form, we bought from is Albany International, NH, USA. The Pi-preform we use, is usually termed "pi-clip" in woven industry, and the one we use is the standard lockheed-martin patented clip with 0.18" insert and 2.74" width. Detailed dimensions are attached (it is not CFRP, it is just carbon fiber, more pictures are attached). Last time we bought it is in 2009, and they had no shipping restrictions, and could not get further from them. I am not sure your company can help me to make some or not. But if you have any information about this kind of pi-from please contact with me. Hope you can help us.



Thanks
http://img.aalun.com/di/B2Z8/QQ20121116-1.png
http://img.aalun.com/di/F6JZ/IMG_0644.jpg
http://img.aalun.com/di/9RTW/IMG_0645.jpg
http://img.aalun.com/di/FM41/IMG_0646.jpg
http://img.aalun.com/di/5U02/IMG_0647.jpg
Edited 13 Years Ago by Zhengning Zhang
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search