I've used it as a print blocker with epoxy/carbon infusion and it is invisible - it just looks like a thicker resin layer.  If you overlap it in places it can be a little yellow-ish or thick looking. Have had pinhole issues with spray-adhesive when putting it in the mold - not sure if type of spray or quantity was at play - wasn't bad but the parts were getting painted.




Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Dezer - 10/22/2019 12:10:34 PM
Lester Populaire - 10/22/2019 6:27:09 AM
placed in mould as a first layer. I am not sure it will become clear enough to use it if you want to show the fabric. i usually use a 30gsm glass fleece which works well in reducing print through.

Thanks for information! 

I've been talking to the manufacturer and they answered me the following:
The Finishmat will give a fully transparent and glossy finish like that of a transparent gelcoat, without having to apply the gelcoat.
The Finishmat is co-infused and this is works very well for a durable carbon look.


Good to know! 

Dezer
Dezer
Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
Lester Populaire - 10/22/2019 6:27:09 AM
placed in mould as a first layer. I am not sure it will become clear enough to use it if you want to show the fabric. i usually use a 30gsm glass fleece which works well in reducing print through.

Thanks for information! 

I've been talking to the manufacturer and they answered me the following:
The Finishmat will give a fully transparent and glossy finish like that of a transparent gelcoat, without having to apply the gelcoat.
The Finishmat is co-infused and this is works very well for a durable carbon look.


Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
placed in mould as a first layer. I am not sure it will become clear enough to use it if you want to show the fabric. i usually use a 30gsm glass fleece which works well in reducing print through.
Dezer
Dezer
Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
Hello, 

There is this product on their Lantor website (Lantor FinishMat D77) , but I never saw any comment about it or see videos being applied.

On the site just says this:

Lantor Finishmat® D77
- Excellent surface finish
- Reduction of process cycle time
- Gelcoat can be replaced by pigmented resin
- Easy to process
- Becomes translucent in resin
- High elongation

Applications Lantor Finishmat® D77
- Marine: hulls, decks, and structures of boats and yachts
- Transportation: parts and panels of cars, trailers,
trucks and RV’s
- General closed mould applications

However I could not understand at what stage of the process is used, if it can be used for those who do infusion without Gelcoat, etc ..