By Dezer - 10/21/2019 11:28:06 PM
Hello,
There is this product on their Lantor website (Lantor FinishMat D77) , but I never saw any comment about it or see videos being applied.
On the site just says this:
Lantor Finishmat® D77 - Excellent surface finish - Reduction of process cycle time - Gelcoat can be replaced by pigmented resin - Easy to process - Becomes translucent in resin - High elongation
Applications Lantor Finishmat® D77 - Marine: hulls, decks, and structures of boats and yachts - Transportation: parts and panels of cars, trailers, trucks and RV’s - General closed mould applications
However I could not understand at what stage of the process is used, if it can be used for those who do infusion without Gelcoat, etc ..
|
By explorecomposites - 11/1/2019 8:06:42 PM
I've used it as a print blocker with epoxy/carbon infusion and it is invisible - it just looks like a thicker resin layer. If you overlap it in places it can be a little yellow-ish or thick looking. Have had pinhole issues with spray-adhesive when putting it in the mold - not sure if type of spray or quantity was at play - wasn't bad but the parts were getting painted.
|
|