So I got my first part out. Cracked few places-I think two layers of 200g 2x2 might be not enough. Fabric moved few places but otherwise than that I'm happy. 
Question time haha:
 I used only EC mould released- can I use 3m 75 glue direct on mould release to hold fabric on sides?