Group: Forum Members
Posts: 2,
Visits: 81
|
Greetings!
Would love to know on your experience and insights on the best possible way to get a flat and even finishes on your carbon fiber projects, especially on hand layup process.
Normally what I did was to spray paint on the surfaces till I get rid of it to get an even finishes. Would love to hear out if your method is different than mine.
Thank you for sharing info's in advance!
|