Abraham George - 8/21/2019 5:10:23 PM
Lester Populaire - 8/21/2019 4:19:13 PM
Or just measure thickness of fabric stack with some calipers and reasonable clamping force. Will get you close. Double check with resin density and fibre density and expected volume fraction. Will get you close as well.

Stack which includes mesh, peel ply....right?

Well no, if you aim for 3mm of glass i personally would use about 3mm of glass...

Abraham George
Abraham George
Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)
Group: Forum Members
Posts: 5, Visits: 7
Lester Populaire - 8/21/2019 4:19:13 PM
Or just measure thickness of fabric stack with some calipers and reasonable clamping force. Will get you close. Double check with resin density and fibre density and expected volume fraction. Will get you close as well.

Stack which includes mesh, peel ply....right?

Abraham George
Abraham George
Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)
Group: Forum Members
Posts: 5, Visits: 7
Greybridge - 8/21/2019 3:29:25 PM
Abraham George - 8/21/2019 1:21:56 PM
So if I want to make a 3 mm thick plate with E-glass reinforcement...what is the approx no of fibre layers we should use? Our is a research proj on vartm based composites so the plate size is of limited dimensions and there is no mould also.

The only way to know for sure is to do a few test runs with a known layer count and a consistent lean out pressure. DO NOT leave your infusion under full vac to lean out. Your resin will boil and and your part will be garbage. Pull resin at full vac until it enters the vent tube, then reduce vac to a lean out pressure appropriate to your tests (go slow so air doesn't push back into your part). Without knowing what your end goal is I can't say exactly what the lean out pressure should be but I wouldn't go more than -15hg. That will get you below the condensation point of your resin and reduce your void volumes by half but still be enough vac to evacuate resin and give you some amount of compaction. Which brings me back to the point, the amount of compaction will affect your per layer thickness. There's a few ways to control this but the most accurate is to weigh your layup before and during infusion and evacuate resin until you hit a specific resin/fabric ratio. Once you have control over your r/f you can predict your mm/layer and thus predict your ultimate part thickness. 

What do you mean by goal?

Lester Populaire
L
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Or just measure thickness of fabric stack with some calipers and reasonable clamping force. Will get you close. Double check with resin density and fibre density and expected volume fraction. Will get you close as well.
Greybridge
G
Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)
Group: Forum Members
Posts: 3, Visits: 50
Abraham George - 8/21/2019 1:21:56 PM
So if I want to make a 3 mm thick plate with E-glass reinforcement...what is the approx no of fibre layers we should use? Our is a research proj on vartm based composites so the plate size is of limited dimensions and there is no mould also.

The only way to know for sure is to do a few test runs with a known layer count and a consistent lean out pressure. DO NOT leave your infusion under full vac to lean out. Your resin will boil and and your part will be garbage. Pull resin at full vac until it enters the vent tube, then reduce vac to a lean out pressure appropriate to your tests (go slow so air doesn't push back into your part). Without knowing what your end goal is I can't say exactly what the lean out pressure should be but I wouldn't go more than -15hg. That will get you below the condensation point of your resin and reduce your void volumes by half but still be enough vac to evacuate resin and give you some amount of compaction. Which brings me back to the point, the amount of compaction will affect your per layer thickness. There's a few ways to control this but the most accurate is to weigh your layup before and during infusion and evacuate resin until you hit a specific resin/fabric ratio. Once you have control over your r/f you can predict your mm/layer and thus predict your ultimate part thickness. 
Abraham George
Abraham George
Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)
Group: Forum Members
Posts: 5, Visits: 7
So if I want to make a 3 mm thick plate with E-glass reinforcement...what is the approx no of fibre layers we should use? Our is a research proj on vartm based composites so the plate size is of limited dimensions and there is no mould also.
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh correct, it depends on the fibre densities. However it does still provide a useful indication.
Lester Populaire
L
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Hanaldo - 8/21/2019 6:10:03 AM
When using woven materials under vacuum compaction, the fibre weight per layer corresponds very closely to the cured thickness. For example, a single layer of 200g woven carbon will provide roughly 0.2mm thickness, a 450g woven carbon will provide roughly 0.5mm thickness, a 650g carbon will provide roughly 0.7mm thickness, etc.

Only accurate for carbon tho. Glass is going to be thinner at the same surface weight, natural fibers are going to be thicker for a given surface weight.

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
When using woven materials under vacuum compaction, the fibre weight per layer corresponds very closely to the cured thickness. For example, a single layer of 200g woven carbon will provide roughly 0.2mm thickness, a 450g woven carbon will provide roughly 0.5mm thickness, a 650g carbon will provide roughly 0.7mm thickness, etc.
Abraham George
Abraham George
Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)
Group: Forum Members
Posts: 5, Visits: 7
I would like to know if there is any particular method to know abt the thickness of the composite before curing. How do you calculate the amt of materials for getting a required thickness in Resin Infusion ?