finishing after infusion


Author
Message
8900120d
8900120d
Supreme Being (308 reputation)Supreme Being (308 reputation)Supreme Being (308 reputation)Supreme Being (308 reputation)Supreme Being (308 reputation)Supreme Being (308 reputation)Supreme Being (308 reputation)Supreme Being (308 reputation)Supreme Being (308 reputation)
Group: Forum Members
Posts: 37, Visits: 939
Hi guys, 
Ive finally got the hang of making moulds and infusing. ive managed to infuse several times, however i get pin holes in the same area everytime, which makes me believe its the mould?

its an automotive part, so it needs to have a nice appearance but it also needs to be protected from the elements. 
i have experimented with XCR :
1. apply 2 coats of XCR
2. sand down with 180 grit until smooth
3. apply 2 coats of XCR 
4. sand down with 240 grit until smooth
5. apply final layer of XCR 
6. sand with 400 - 800 grit
7. polish

however everytime i apply a layer of XCR, by the time it becomes tacky it has loads of "craters" (see pic) 
it feels like a never ending process to get it smooth again and then apply another layer which again has craters when it drys!

the reason why i use XCR is to get hide of the pin holes and small dry spots in the corners on the finished product
but its an extremely long process! especially if i decide to sell this part.

is there a quicker method of using resin clear coat which will get rid of a small amount of pin holes and dry areas?

for e.g; can i apply 2 layers of XCR, sand down with 180 grit, and then spray some automotive clear coat ontop?



 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
8900120d - 6 Years Ago
Fasta - 6 Years Ago
MarkMK - 6 Years Ago
8900120d - 6 Years Ago
oekmont - 6 Years Ago
8900120d - 6 Years Ago
oekmont - 6 Years Ago
8900120d - 6 Years Ago
oekmont - 6 Years Ago
8900120d - 6 Years Ago
MarkMK - 6 Years Ago
oekmont - 6 Years Ago
MarkMK - 6 Years Ago
8900120d - 6 Years Ago
MarkMK - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search