Size problems skinning hood 160cm


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)Supreme Being (30K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You would be best to use a stabilised fabric such as our ProFinish Carbon Fibre 2/2 Twill 3k 210g as it is much easier to cut.  It is easier to make a feature of the join line by doing it in the middle for example. You could add strips of carbon tape as a feature line or as I have seen in a few cases recently, a thicker stripe of a Textreme or Spread tow fabric similar to our Carbon Fibre Spread-Tow 15mm Plain Weave.  That way it looks like it has been done that way by design. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
368wraps
3
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 3, Visits: 93
Hello, I  will do skinning carbon fiber on hood, the problem will be , hood size 2000mm X 1600mm,
Im thinking do in two pieces, but the cut is very difficult . I m prefer do in one piece .
Something idea? The biggest size are 1500mm
Thanks, sorry my english is bad