Why cant i get the corners right! (see picture)
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
8900120d
8900120d
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 37,
Visits: 939
Hi guys,
ive done a few infusions now, but im struggling to get the corners right!
- Perfectly sealed bag
- everything is room temp
- i tuck the bag in all of the edges
- use an edge peice to push all of the corners in
- all of the resin is degassed
i always end up with corners bad corners!
im using the FM100 mesh and i feel like it doesnt 'tuck' into the corners properly even after the bag has been pressurised
should i be using mesh on the corners?
is there a way of fixing the corners after the infusion?
thank you
Edited
6 Years Ago by
8900120d
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Why cant i get the corners right! (see picture)
8900120d
-
6 Years Ago
Not always easy to tell from pictures, but the overall finish of your part doesn't look great, despite the evidence of the resin surface being broken away after de-mould. Did the infusion go okay wit...
MarkMK
-
6 Years Ago
Thank you for your detailed response! The infusion went well as far as im aware. i like the idea of cutting the fabric in the corners and jointing, however im afraid spray tack might ruin the...
8900120dd
-
6 Years Ago
Well.laid sections will often look much better than a single piece with weave distortion, even if the join is visible so this might be a better approach. I can only comment on using Cytec's Aerofix ...
MarkMK
-
6 Years Ago
thank you for your response. would you guys recommend using Knitted mesh for moulds with very tight corners?
8900120d
-
6 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search