	Group: Forum Members 	        
    Posts: 550, 
    Visits: 27K 
    
 
          
		     | 
				                       
                 
                
                    
			            This isn't really an application for epoxy+carbon. There are some briefcases wich are partial made from flexible carbon fibre. These are made from flat sheets of carbon fibre cloth in a transparent silicone matrix. From there on you could use it to some degree like regular cloth to tailor things.                 
			            				
			                                 
                     
                                            
                         
                    
                  
             |