Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Epoxy putty
Epoxy putty
Post Reply
Like
3
Epoxy putty
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
alex3horse
a
alex3horse
posted 6 Years Ago
ANSWER
HOT
Topic Details
a
Group: Forum Members
Posts: 2,
Visits: 10
Hi which type of epoxy is best for mixing with fillers please? Without lots of smelly fumes too
Thanks
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Epoxy putty
alex3horse
-
6 Years Ago
It entirely depends what you are trying to achieve. Vast majority of epoxies are very low odour anyway.
Warren (Staff)
-
6 Years Ago
Thanks Warren 😊 I'm casting with it, making sculptures. I mixed west system epoxy with sawdust and silica. I've never used epoxy before so want to make sure I've got the right stuff for the job....
alex3horse
-
6 Years Ago
As long as you use a slow hardener and quite a good quantity of filler powders, then you should be ok. The danger with fillers like this is excessive exotherm if the heat does not dissipate - eg you....
Warren (Staff)
-
6 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search