Pump failed during an initial low-temp cure cycle using the XT135 Tooling prepreg.(400mm diameter x 22mm part size)
I have emptied out the oil and it is a dark brown colour.(no metal checked with a magnet) The pump is seized however the motor seams to want to turn.
Order the pump on 13/05/2019 and has been used three times.

Warren (Staff)
Warren (Staff)
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Sorry to hear your pump has failed. Sounds like something has majorly gone wrong with the pump for it to stop working like that.  As the pump is still under warranty we would recommend you return it to us and we will investigate for repair or replacement.

From your account details I cannot find your order, can you message me or email us on technical@easycomposites.co.uk with your order number and I will put a note on to expect your pump back for repair or replacement.  Also please put a note in the box so we know that the pump is yours.

Hopefully we can get this sorted for you quickly and get you back up and running.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
flamano
flamano
Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)
Group: Forum Members
Posts: 10, Visits: 141
Warren (Staff) - 6/12/2019 10:38:41 AM
Sorry to hear your pump has failed. Sounds like something has majorly gone wrong with the pump for it to stop working like that.  As the pump is still under warranty we would recommend you return it to us and we will investigate for repair or replacement.

From your account details I cannot find your order, can you message me or email us on technical@easycomposites.co.uk with your order number and I will put a note on to expect your pump back for repair or replacement.  Also please put a note in the box so we know that the pump is yours.

Hopefully we can get this sorted for you quickly and get you back up and running.

Thank you for your reply,
My Order No #217329

Warren (Staff)
Warren (Staff)
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
No Problem, thanks for that.  I have also responded to your email. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
flamano
flamano
Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)
Group: Forum Members
Posts: 10, Visits: 141
Warren (Staff) - 6/12/2019 10:54:06 AM
No Problem, thanks for that.  I have also responded to your email. 

May I confirm the return address to be,  Unit 39, Park Hall Business Village, Longton, Stoke on Trent, ST3 5XA

Warren (Staff)
Warren (Staff)
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
That is correct.  Soon as the pump arrives, our engineer will do some tests to determine the fault.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
flamano
flamano
Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)
Group: Forum Members
Posts: 10, Visits: 141
Hello,
Pleases may I receive an update regarding the pump?
Warren (Staff)
Warren (Staff)
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Your pump is still being tested as we speak.  Hopefully the tests and diagnosis will be complete sometime tomorrow, at which point we will be able to email you with a report and a way forward. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Warren (Staff)
Warren (Staff)
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi,

Our engineer has now completed the testing of the pump.  I have emailed you the full report.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
flamano
flamano
Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)Supreme Being (143 reputation)
Group: Forum Members
Posts: 10, Visits: 141
I have not received the email.
Please can you resend to guzzettilimited@gmail.com
Thankyou
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search