Best vacuum pump for a reasonable price?
Best vacuum pump for a reasonable price?
Post Reply
Like
6
Best vacuum pump for a reasonable price?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
oekmont
oekmont
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 550,
Visits: 27K
This is a dual stage pump, which isn't necessary for composite applications. A cheaper single stage pump will work just as fine
Reply
Like
6
JasonFL
JasonFL
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 51,
Visits: 707
Robinair 15500 will pull full vacuum depending on what altitude you’re at
Jason
Reply
Like
7
oekmont
oekmont
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 550,
Visits: 27K
As long as you want to do anything but wet layup without vacuum compression, you will need a vacuum pump. For beginners almost any rotary vane pump (oil bath) will do the job. You can get a great variety at Amazon and eBay.
Reply
Like
7
Turkey
T
Turkey
posted 7 Years Ago
ANSWER
HOT
Topic Details
T
Group: Forum Members
Posts: 1,
Visits: 9
Hello, I'm really new to this carbon fiber parts making using vacuum pump, so I was wondering if you guys know what would be the best vacuum pump for a reasonable price (). Or vacuum pump is not necessary if you are new to carbon fiber parts making?
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search