Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Best vacuum pump for a reasonable price?
Best vacuum pump for a reasonable price?
Post Reply
Like
11
Best vacuum pump for a reasonable price?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
oekmont
oekmont
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 550,
Visits: 27K
This is a dual stage pump, which isn't necessary for composite applications. A cheaper single stage pump will work just as fine
Reply
Like
10
JasonFL
JasonFL
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 51,
Visits: 707
Robinair 15500 will pull full vacuum depending on what altitude you’re at
Jason
Reply
Like
12
oekmont
oekmont
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 550,
Visits: 27K
As long as you want to do anything but wet layup without vacuum compression, you will need a vacuum pump. For beginners almost any rotary vane pump (oil bath) will do the job. You can get a great variety at Amazon and eBay.
Reply
Like
12
Turkey
T
Turkey
posted 7 Years Ago
ANSWER
HOT
Topic Details
T
Group: Forum Members
Posts: 1,
Visits: 9
Hello, I'm really new to this carbon fiber parts making using vacuum pump, so I was wondering if you guys know what would be the best vacuum pump for a reasonable price (). Or vacuum pump is not necessary if you are new to carbon fiber parts making?
Reply
Like
11
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
11
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions