			            Hi Im currently making a large foam mould for uses as a nose cone for a small single seat racing car.  
  We have used Easy Composites Low Density polyurethane foam to fill in gaps between our MDF skeletal frame. I would like to make sure that I have the process correct for creating the mould as I only have one shot at this.
  For the Plug once sanded body filled and completely finished i'll paint on a layer of EG60 Epoxy tooling gelcoat and allow this to fully cure, then apply at least 6 layers of the Easy-Lease Chemical release agent, followed by at least 2 layers of mirror glaze mould release wax. 
  Then im using 4 layers of 100gsm CSM fibre glass to create the mould from which I can infuse upon.
  Is this process correct or is there anywhere I should make alterations please let me know.