You can use lots of different materials for compression moulding. The Americans have been using bmc and smc composites since the 50s. I've done some stuff with prepreg and chopped prepreg similar to the quantum material.
Vtc401 from shd materials processes in a heated press. Iirc it's 150degrees for 15mins.
|