The ideal stage to cast the P6 to ensure adequate bonding would be to pour it at the firm but tacky stage of the cure. The PU in the P6 should then cross link and bond to the PX30. However it would be worth experimenting with your specific application as it is possible the soft flexible surface coating may peel or be able to tear off the rigid P6 surface if the bond is not that strong. What is the application?
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|