Group: Forum Members
Posts: 2,
Visits: 9
|
Hi I used Glass Cast 3 for my mosaic table top project. I followed the instructions measured and mixed the the resin. Once I poured it I left it to set for 48 hours. The resin had set well and was clear so I took the table top outside. The following morning I noticed some white wavey lines had appeared in the resin. Picture attached. I was wondering if there was a way to get rid of these lines.
|