			            Unfortunately once the resin has fully cured, it is not possible to soften it with heat without damaging it.  You can sand that area to remove the defect and then refill with fresh resin.  You will then need to sand the surface level to get it to match nicely and if the hole you had to dig is particularly deep you may need to overcoat the area with resin to bring the level back up to where it needs to be.   The key thing is what ever tools or sandpapers you use, it is critical to ensure the resin is properly cleaned afterwards to ensure no dust or dirt gets trapped when re-pouring.
 