Hi
I used Glass Cast 3 for my mosaic table top project. I followed the instructions measured and mixed the the resin. Once I poured it I left it to set for 48 hours. The resin had set well and was clear so I took the table top outside. The following morning I noticed some white wavey lines had appeared in the resin. Picture attached.
I was wondering if there was a way to get rid of these lines.
Attachments
20190402_190231.jpg (529 views, 3.00 MB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search