Hi all,
My question is the 100:5 mixing ratio, is it whatever the weight is eg: 170g of silicone part A  X  5% of catylist   
So 170g x 5% = 8.75 catalyst? 
Thanks for any help.
Sean

Rich (Staff)
Rich (Staff)
Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Spot on yes; for every 100g of Silicone, you need 5g of catalyst and transposing this, you need 8.5g of catalyst for 170g of Silicone part A.

There are various ways to work this out and everyone has their own favourite, my personal preference is as follows because it uses all of the numbers at hand and also works where a ratio isn't 100:XX, (using your example):

(170 / 100) x 5 = 8.5g 
but
5% in this case works just as well.
Edited 7 Years Ago by Rich (Staff)
S34n
S
Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)
Group: Forum Members
Posts: 18, Visits: 54
Rich (Staff) - 3/13/2019 11:34:36 AM
Spot on yes; for every 100g of Silicone, you need 5g of catalyst and transposing this, you need 8.5g of catalyst for 170g of Silicone part A.

There are various ways to work this out and everyone has their own favourite, my personal preference is as follows because it uses all of the numbers at hand and also works where a ratio isn't 100:XX, (using your example):

(170 / 100) x 5 = 8.75g 
but
5% in this case works just as well.


Thank you Rich thats great, felt like a bit of a dumb pleb asking this question but you managed to help me keep my dignity....w00tLaughBigGrinBigGrinBigGrinBigGrinBigGrin
Rich (Staff)
Rich (Staff)
Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)Supreme Being (1.5K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
No such thing as a stupid question other than the one which is never asked!!
S34n
S
Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)
Group: Forum Members
Posts: 18, Visits: 54
Rich (Staff) - 3/13/2019 3:19:30 PM
S34n - 3/13/2019 2:29:13 PM
Rich (Staff) - 3/13/2019 1:45:37 PM
No such thing as a stupid question other than the one which is never asked!!


Well in that case, BigGrin when I put your method :- (170 / 100) x 5 = 8.75g   Into a calculator it shows 8.5 how did you get 8.75?

oops; yes, 8.5 - my bad!!



So my bad then...BigGrinw00tLaugh
Thank god for that I thought I was going mad, you have no idea how many times and different ways  I wrote it into the calculator....BigGrinLaughBigGrinLaugh anyway thank you so much for your help 
thank you Rich                                

Edited 7 Years Ago by S34n
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search