Unfortunately the GlassCast range of resins are not designed or suitable for the level of water immersion and exposure found within a shower tray or wet room. The resin would be quickly degraded in such a situation. At present we do not have any clear casting resins suitable for such purpose.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|