By SVant - 3/5/2019 9:16:03 AM
Hi, I am wanting to make a pebble effect shower tray. I was intending to pour your glass cast 50 over washed pebbles to create a ~50mm thick shower tray with a river-bed pebble look. I will jig it initially at a slight incline and then tip it back when fully cured to create a run-off slope to the drain. Can you forsee any issues or have any suggestions? Also would doing a top layer of glasscast 3 create a more durable finish? Regards
|
By Warren (Staff) - 3/5/2019 2:59:18 PM
Unfortunately the GlassCast range of resins are not designed or suitable for the level of water immersion and exposure found within a shower tray or wet room. The resin would be quickly degraded in such a situation. At present we do not have any clear casting resins suitable for such purpose.
|
|