Rossion Q1


Author
Message
hunterisgreat
h
Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)
Group: Forum Members
Posts: 8, Visits: 254
This will be where I'll document the progress slowly but steadily replacing parts on my Rossion Q1 in the never ending quest to add lightness. The car currently makes about 600hp at full boost, weighs about 2400lbs. I have/had zero experience starting this project so prepare for less than flawless parts early on... already made several dumpster parts. Successfully made some under-hood covers for the backs of the headlight pods.. trying to make replacement headlight pods now but its a pretty complex shape. I'll upload some more pics soon

Here is the car.



andygtt
andygtt
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
hunterisgreat - 3/2/2019 4:08:17 PM
This will be where I'll document the progress slowly but steadily replacing parts on my Rossion Q1 in the never ending quest to add lightness. The car currently makes about 600hp at full boost, weighs about 2400lbs. I have/had zero experience starting this project so prepare for less than flawless parts early on... already made several dumpster parts. Successfully made some under-hood covers for the backs of the headlight pods.. trying to make replacement headlight pods now but its a pretty complex shape. I'll upload some more pics soon

Here is the car.



Hi, Good luck with the project.... I remade every single panel on my Noble M12 in carbon so if you want any advice drop me a line Smile

I made the headlight buckets using something called Alusil, that is basically a fibre coated in alloy and weaved in a similar pattern to carbon... looks great and helps the lights project Smile