Group: Forum Members
Posts: 550,
Visits: 27K
|
Of course there is. The resin uptake for soric is very well documented. Here the numbers out of my main supplier's catalogue, wich are within +-10% to my experiments: Resin uptake in kg/m^2: Sf2mm: 1 sf3mm: 1,3 lrc1,5mm: 0,6 lrc2mm: 0,8 lrc3mm: 1 from here the actual volumetric resin contend is just one simple calculation away. But I don't know why you want to know that, except to calculate the resin uptake.
|