As I watch many tutorials, I see some tutorials that use breather/bleeder fabric and other tutorials that use none at all. What factors influence the choice to use or not use it? For reference, my projects will all be small projects from 0.10 square meter to about 1 square meter. The shapes will be quite simple and relatively flat with only modest curves.