Hi guys. I've just poured my first river table with some nice oak. I Maybe didn't leave enough time between pours as the temperature is 13/14 degrees. It was probably too sticky still. Anyways its shrunk and I need more resin to Complete the table. It's my first time ever working with resin. If anyone has tips about pouring onto an already cured river would be greatly appreciated. Be it sanding etc. Thanks, Daniel 
Reply
Dsully
D
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 5, Visits: 19
Bhamoggy - 2/3/2019 6:12:46 PM
I had a similar issue a few weeks back so you should be able to find my post easy enough. Temp should be 20 degrees for glasscast 50. Will be fine though so just scratch it up with some 240 grit paper

Thanks for your response mate. Temperature not convenient alright its averaging around 14. Its under my house so have no choice really. Next one will be better. 240 grit it isπŸ‘ŒπŸ‘ŒπŸ‘πŸ‘

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dsully - 6 Years Ago
Bhamoggy - 6 Years Ago
Dsully - 6 Years Ago
Rich (Staff) - 6 Years Ago
Dsully - 6 Years Ago
Dsully - 6 Years Ago
Warren (Staff) - 6 Years Ago
             Cheers mate
Dsully - 6 Years Ago
Graham Burdett - 4 Years Ago
Warren (Staff) - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search