Any silicone hose of the right diameter should be fine.
Lester Populaire
L
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
quinn - 2/1/2019 5:48:38 PM
oekmont - 2/1/2019 3:48:58 PM
The only thing I can really think of wich is accessible everywhere would be brake tubing for cars. Obviously not optimal in any way, but possible. Or you search for a pneumatic supplier nearby, to get something wich is made for this application. Usually a silicone hose.

Ok I'll have a look around. I could probably even come straight into the oven with a peice of copper tube to connect to the pressure inlet of the bladder. If I don't find a good solution and end up having to order, what is the proper stuff?

We get the pressure lines made by an car shop that makes brake lines. The ones we get are good for up to 260° C and work really well.

quinn
q
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 155, Visits: 992
oekmont - 2/1/2019 3:48:58 PM
The only thing I can really think of wich is accessible everywhere would be brake tubing for cars. Obviously not optimal in any way, but possible. Or you search for a pneumatic supplier nearby, to get something wich is made for this application. Usually a silicone hose.

Ok I'll have a look around. I could probably even come straight into the oven with a peice of copper tube to connect to the pressure inlet of the bladder. If I don't find a good solution and end up having to order, what is the proper stuff?

oekmont
oekmont
Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
The only thing I can really think of wich is accessible everywhere would be brake tubing for cars. Obviously not optimal in any way, but possible. Or you search for a pneumatic supplier nearby, to get something wich is made for this application. Usually a silicone hose.

quinn
q
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 155, Visits: 992
Im about ready to try a bladder in my mold. First one went pretty well with vacuum, but the line melted at about 110c. Luckily it kind of just collapsed on itself and sealed so part came out fine, but I obviously need something better. Is there something I can get at the hardware store that will hold up to 120c? I'm sure I could order something, but really want to lay up a part this weekend. Might be doing both vacuum and pressure so preferably something that will work for either.