	Group: AdministratorsPosts: 2.5K, 
    Visits: 8.5K
 
 | 
                    
			            As long as you sand deep enough to eliminate the bubbles so it all fills with fresh resin then you should be fine.  The fresh resin will fill in all the scratches and make it a glossy finish again.  Ensure the piece is as clean as possible before pouring the next layer of resin as otherwise any dirt will be trapped and stand out. 
 