Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Resin Casting and Moulding Forum
»
Clear Casting and Coating
»
GlassCast 3 - Bubble Disaster
GlassCast 3 - Bubble Disaster
Post Reply
Like
3
GlassCast 3 - Bubble Disaster
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
MrZeeba
M
MrZeeba
posted 7 Years Ago
ANSWER
HOT
Topic Details
M
Group: Forum Members
Posts: 1,
Visits: 47
Hi Everyone,
So to cut a long story short. I foolishly didn't seal my wood before going ahead with pouring my 3mm layer on for a desk I'm making. As the resin thickened more and more bubbles kept cropping up and I attempted to battle them off with my trusty heat gun...but in the end the resin became too thick for the bubbles to escape as the wood just kept releasing them.
Anyway, no need to cry over spilt milk. I'm trying to recover the project now and I'm looking for some help/advice to recover it.
So the current state of play is that I have bubbles all over the place. (see very embarrassing image above).
I was thinking what I'd do is first sand the whole thing down to get open up the bubbles, then add another 1mm layer over the top of the whole thing. I'm unsure as to whether the extra layer would actually hide the scratches I'd make by sanding the whole thing?
And whether I'm actually going about the right way of fixing it.
Any opinions/advice would be appreciated. Thanks!
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
GlassCast 3 - Bubble Disaster
MrZeeba
-
7 Years Ago
As long as you sand deep enough to eliminate the bubbles so it all fills with fresh resin then you should be fine. The fresh resin will fill in all the scratches and make it a glossy finish again....
Warren (Staff)
-
7 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search