Outgassing / Boiling of IN2 Infusion Resin


Author
Message
philiplardner
philiplardner
Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)Supreme Being (656 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
I've just infused my first test piece, a carbon/foam sandwich using your IN2 Infusion Resin and I am seeing *a lot* of outgassing from the resin under full vacuum. Small bubbles are visable within the within the resin transfer mesh and continue to form/appear as long as there is a hard vacuum. Will this compromise the strength or the cosmetic finish of the finished part? (I haven't de-molded yet.) Is there any way to elimitate outgassing?

Thanks,

Phil.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search