By philiplardner - 1/29/2012 12:32:48 AM
I've just infused my first test piece, a carbon/foam sandwich using your IN2 Infusion Resin and I am seeing *a lot* of outgassing from the resin under full vacuum. Small bubbles are visable within the within the resin transfer mesh and continue to form/appear as long as there is a hard vacuum. Will this compromise the strength or the cosmetic finish of the finished part? (I haven't de-molded yet.) Is there any way to elimitate outgassing?
Thanks,
Phil.
|
By philiplardner - 1/30/2012 12:28:53 PM
I've just been out to the workshop and the vacuum gage has dropped from -1bar to around -.8 overnight... so I do have a leak after all. I only did a short (5-10min) vacuum check before introducing the resin (impatients I guess.) Lesson learned - I'll perform a full 30min vacuum integrety test in future.
Apologies, mea culpa!