You can even get 300mm tubing at amazon. In Germany you have to search for "kg rohr dn300". Every good hardware store should get their hands on that dimension. This is used in every bigger building.
If you do the plug with primer etc, you should definitely try to get a good finish on the plug. There is too much danger of sanding through the gelcoat.

Robert72
R
Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)
Group: Forum Members
Posts: 57, Visits: 151
I would indeed have used a plastic tube for cheap money if I could get one where I live.  Unfortunately all I can get hold of is a 3m length of Sonotube, however it is incredibly straight and round.  I think I follow you now, making a mould and then finishing it post cure, rather than polishing up the plug. Good idea.  It is difficult for me to follow sometimes as this is my first project, and I am therefore erring on the safe side of assuming the plug has to finished to a very high standard etc.  Thanks for your input, it is appreciated.
oekmont
oekmont
Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
You want to take a negative mould from a 295mm cardboard tube, wich you want to cover with glass fibre until it's 300mm diameter, right? To finally make a carbon tube, right. I would not use an enlarged cardboard tube, but a tube, wich you can get a better hardware stores for cheap money instead. Because it is plastic and hard to polish up nicely, I would instead take the mould from the raw tube, and sand and polish the mould afterwards. Because the surface is already quite good, that would not take long, and the should be no danger to sand through the tooling coat. In the end you will safe much money and even more time. And you'll get a a better finish.

Robert72
R
Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)
Group: Forum Members
Posts: 57, Visits: 151
Sorry oekmont I am completely baffled.
oekmont
oekmont
Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
In my opinion this is far to complicated and unnecessary expensive. And will likely result in an uneven surface. It is quite difficult to sand a tube perfectly round without a jig.
I would take a kg type tube (used in plumbing) wich you can get at 300mm diameter and 1,5m length. The finish isn't that great, but it's straight and even. Wich will be hard to achieve with your method. Then take the mold, remove the tube, trim the edges and close the mould again. In this closed state, start sanding the mould beginning with 400grit. This ensures, that your flange edges stay sharp. Then use high grits. 800, 1000, 1500 and finally 2000. Finally take the mould apart and polish it up to high gloss. This will give you a nice finish.

Edited 7 Years Ago by oekmont
Robert72
R
Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)
Group: Forum Members
Posts: 57, Visits: 151
Thank you again for your reply.  Yes it is a card tube:



The diameter is 295mm.  My intention is to build it up to 300mm with woven glass (for various reasons). then prime it with pattern coat primer and high gloss then polish and create a female mould with flanges running down both sides.  If I am using woven glass do I still need the primer and high gloss?  Oekmont, is there a better way of making the mould, sorry I didn't quite understand your description?
oekmont
oekmont
Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Is it a simple tube? If so, I would get a 300mm brown kg type tube (kanal grundrohr in german) and take a would from it, using a melamine coated board as temporary flanges. And then just sand the closed mould beginning with 400 grit and polish each half separately.
That's far less than 100£. You could get away with little over 50£. You could try to buy 1 small kit and 1small of each gelcoat, coupling coat, tooling resin and help and csm. you don't need a second roller. if you need more than half the resin for the first half, you could reorder before starting the second. But I would say you should buy 2 of each from the beginning.

Robert72
R
Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)
Group: Forum Members
Posts: 57, Visits: 151
The area per side is 0.8 sqm.  Do you think I could stretch the 0.7 sqm in the small size kit to this size?  It may be worth considering.
Robert72
R
Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)Supreme Being (765 reputation)
Group: Forum Members
Posts: 57, Visits: 151
The tube is 1.5m x 0.3m, unfortunately just a bit too big for a small kit per side.  I have worked out that to finish the plug (sonotube), the parts come to £227.64, this includes a laminate skin, pattern coat, polish etc.  Add the £314.40 for the large kit and that is £542.04.  I could save a bit of money by using 3 small kits, but for all I would save I might as well get the large.

oekmont
oekmont
Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)Supreme Being (7.9K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
What for an telescope are you building? Something mounted in a medium sized building? With the big starter kit you could definitely build quite a huge telescope mould. Usual mirror telescopes should be even possible with the small kit. and that's 260/80£. Unless you are cnc'ing the plug out of epoxy board, that should be far less than 600£ in total