Group: Forum Members
Posts: 550,
Visits: 27K
|
Is it a simple tube? If so, I would get a 300mm brown kg type tube (kanal grundrohr in german) and take a would from it, using a melamine coated board as temporary flanges. And then just sand the closed mould beginning with 400 grit and polish each half separately. That's far less than 100£. You could get away with little over 50£. You could try to buy 1 small kit and 1small of each gelcoat, coupling coat, tooling resin and help and csm. you don't need a second roller. if you need more than half the resin for the first half, you could reorder before starting the second. But I would say you should buy 2 of each from the beginning.
|