I'm looking to join two matching 3d shaped carbon fiber sheets together with M4 screws and threaded inserts (the threaded insert can't stick out on either side) and I need a few hundred of those holes...
The stack I will drill through is: one sheets is 1mm carbon and glass and the other is 1.5mm carbon, 5mm solid epoxy (core), 1.5mm glass.
The shape is not flat so a drillpress is not an option. The space for a drill cup is also probably to small. But on the other hand perfect 90 degree holes are not necessarily needed. It might also be hard/inconvenient to strap a waste board on the backside to prevent chip-out/blowouts because of the shape
So my question is how do I tackle this the best possible way? I guess making a jig to locate and clamp down the two pieces in place. Find a suitable M4 drillbit that lasts, ideally one that doesn't produce blow-outs and is self starting Drill through both sheets. Enlarge the hole in the thicker carbon piece and find a suitable threaded insert. Hum...
|